Low dosage of ethylene oxide is used. Ethylene oxide can swell most seal materials.
Best Choices
Peroxide cured EP and Silicones can be used since low exposure to Ethylene oxide is normal for the sterilization process.
Low dosage of ethylene oxide is used. Ethylene oxide can swell most seal materials.
Peroxide cured EP and Silicones can be used since low exposure to Ethylene oxide is normal for the sterilization process.
*To request a sample, a quote or to speak with an engineer, please use one of the following forms: Sample Request, Request for Quote or Engineering Requests.
To search our o-ring inventory, please use our O-Ring Size Search tool.
For all other questions…