This class of o-rings is primarily utilized in hydraulic tubing and fittings up to 3000 psi. A straight thread, not tapered, is used so that the o-ring seals under compression. Because of their use in primarily high pressure applications, these seals are normally supplied in 90 durometer material.

O-Rings for Straight Thread Tube Fitting Bosses