LSR Color Solutions

lsr colors

Apple Rubber offers advanced liquid silicone rubber (LSR) pigmentation expertise for color matching and superior quality manufacturing.

LSR Pigmentation Overview

Liquid silicone rubber naturally appears in a range from crystal clear to opaque white. Through our advanced pigmentation process, we can achieve virtually any desired color while maintaining the material's exceptional physical properties. This is accomplished by incorporating just 1-3% pigment into the LSR base material.

Key Pigmentation Specifications

Color Applications

Our color solutions serve multiple practical and aesthetic purposes:

Important Note: Clear LSR may experience slight yellowing over time. Consider this factor when selecting materials for long-term applications.

lsr seal types

Manufacturing Excellence

Our state-of-the-art manufacturing process incorporates concentrated color paste as a third stream while LSR flows into the press. This technique ensures uniform tinting before the molding and curing process begins, resulting in consistent coloration throughout the entire part.

Color Mixing Formula:

98% Liquid Silicone Rubber + 2% Color Paste = 100% Tinted LSR

Advanced Color Measurement Technology

Apple Rubber utilizes the sophisticated CAPSURE® color meter for precise Pantone system matching. This advanced device provides access to:

Our color testing is conducted on standardized 6″ x 6″ x 0.080″ specimens using Silopren™ LSR 2070 (70 shore A durometer) with 2% color paste to ensure consistent results.

Comprehensive Color Solutions

With our extensive portfolio of over 70 color options and custom matching capabilities, Apple Rubber delivers expert solutions for all your LSR coloring requirements. Our experienced team specializes in:

PSTE Black

PSTE Black Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
220
Pantone
20-0196
R: 28
G: 28
B: 27
Pigment Black 11
(Black Iron Oxide)
1317-61-9 35 - 40
297
Pantone
20-0200
R: 24
G: 24
B: 26
Pigment Black 7
(Carbon Black)
1333-86-4 5 - 10
31411
Pantone
Black 4C
R: 49
G: 38
B: 29
Pigment Black 11
(Black Iron Oxide)
1317-61-9 ~ 25
MED NSHCV7199A
Pantone
20-0200
R: 24
G: 24
B: 26
Pigment Black 28
(Copper Chromite)
68186-91-4 40
MED-4900-2
Pantone
Black 7 C
R: 61
G: 57
B: 53
Pigment Black 11
(Black Iron Oxide)
1317-61-9 37
MED50-4900-2 (Translucent)
Pantone
20-0196
R: 28
G: 28
B: 27
Pigment Black 11
(Black Iron Oxide)
1317-61-9 1.11

PSTE Gray

PSTE Gray Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
11C
Pantone®
Cool Gray 11 C
R: 83
G: 86
B: 90
Blend of
Pigment White 6, Pigment Black 7, Pigment Blue 29, & Pigment Red 101
(Titanium Dioxide, Carbon Black, Sodium Aluminum Sulfo Silicate, & Red Iron Oxide)
13463-67-7
1333-86-4
57455-37-5
1309-37-1
~ 28
122
Pantone®
Cool Gray 9 C
R: 117
G: 120
B: 123
Blend of
Pigment Black 11 & Pigment White 6
(Black Iron Oxide & Titanium Dioxide)
1317-61-9
13463-67-7
< 60
174
Pantone®
14-6305 TPX
R: 198
G: 192
B: 177
Blend of
Pigment White 6, Pigment Black 11, Pigment Red 101 & Pigment Yellow 42
(Titanium Dioxide, Black Iron Oxide, Red Iron Oxide & Yellow Iron Oxide)
13463-67-7
1317-61-9
1309-37-1
51274-00-1
~ 42
31451
Pantone®
18-0503 TCX
R: 104
G: 103
B: 103
Blend of
Pigment White 6, Pigment Black 11, Pigment Orange 36 & Pigment Yellow 42
(Titanium Dioxide, Black Iron Oxide, Benzimidazole Orange & Yellow Iron Oxide)
13463-67-7
1317-61-9
12236-62-3
51274-00-1
~ 40
34331
Pantone®
422 C
R: 158
G: 162
B: 162
Blend of
Pigment Black 11, Pigment White 6, & Carbon Black
(Black Iron Oxide, Titanium Dioxide, & Carbon Black)
1317-61-9
13463-67-7
1333-86-4
5 – 10
35 – 40
0 - 5
35022
Pantone®
18-0601 TPG
R: 110
G: 110
B: 109
Blend of
Pigment Green 50 &
Pigment White 6
(Cobalt Titanate & Titanium Dioxide)
68186-85-6
13463-67-7
5 – 10
10 - 25
50792
Pantone®
14-4104 TPG
R: 189
G: 192
B: 191
Blend of
Pigment Blue 28, Pigment White 6 & Carbon Black
(Cobalt Aluminate, Titanium Dioxide, & Carbon Black)
1345-16-0
13463-67-7
1333-86-4
0.3 – 1
25 – 50
0 – 0.3
83193
Pantone®
17-0610 TPG
R: 140
G: 139
B: 124
New Formulation Needed X X
MED1-4900-11
Pantone®
4177 C
R: 187
G: 190
B: 174
Blend of
Pigment White 6, Pigment Orange 64, Pigment Black 11 & Pigment Yellow 138
(Titanium Dioxide, 2,4,6(1H,3H,5H)-Pyrimidinetrione,5-[(2,3-dihydro-6-methyl-2-oxo-1H-benzimidazol-5-yl)azo]-, Black Iron Oxide & Quinophthalone Yellow and Lithol Fast Yellow 1090)
13463-67-7
72102-84-2
1317-61-9
30125-47-4
25 – 50
5 – 10
< 30
< 20
093A
Pantone
7540 XG C
R: 76
G: 80
B: 88
Blend of
Pigment White 6 & Pigment Black 11
(Titanium Dioxide & Black Iron Oxide)
13463-67-7
1333-86-4
10 ≤ X ≤ 25
5 ≤ X ≤ 10

PSTE White

PSTE White Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
056
11-0501
Baby Powder
R: 247
G: 246
B: 238
Pigment White 6
(Titanium Dioxide)
13463-67-7 < 50
239
Pantone
12-0105 TPG
R: 222
G: 215
B: 195
Blend of
Pigment White 6,
Pigment Red 101,
Pigment Yellow 42, &
Pigment Black 11
(Titanium Dioxide, Red Iron Oxide, Yellow Iron Oxide & Carbon Black)
13463-67-7
1332-37-2
20344-49-4
1317-61-9
40 – 45
0 – 5
0 – 5
0 - 5
244882
11-0501
Baby Powder
R: 247
G: 246
B: 238
Pigment White 6
(Titanium Dioxide)
13463-67-7 30 < X < 60
Med NSHCV9052A
Pantone
11-4202 TCX
R: 239
G: 239
B: 232
Pigment White 6
(Titanium Dioxide)
13463-67-7 45
Med NSHCV9086A
Pantone
12-0105 TPG
R: 245
G: 235
B: 208
Pigment White 6
(Titanium Dioxide)
13463-67-7 20 ≤ X < 50
Med-4900-1 (Translucent)
Pantone
11-0602 TPG
R: 240
G: 237
B: 230
Pigment White 6
(Titanium Dioxide)
13463-67-7 25 - 50
Med 50-4900-1 (Translucent)
Pantone
413 C
R: 186
G: 187
B: 177
Pigment White 6
(Titanium Dioxide)
13463-67-7 < 5

PSTE Brown

PSTE Brown Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
159A
Pantone
4625 C
R: 79
G: 44
B: 29
Blend of
Pigment Red 101, Pigment Yellow 42, & Carbon Black
(Red Iron Oxide, Yellow Iron Oxide & Carbon Black)
1332-37-2
51274-00-1
1333-86-4
15 – 20
5 – 10
0 - 5
54362
Pantone
4272 C
R: 126
G: 106
B: 93
New Formulation Needed X X
67497
Pantone
7497 C
R: 122
G: 114
B: 86
Blend of
Pigment Orange 64, Pigment White 6, Pigment Red 254, & Pigment Green 50
(2,4,6(1H,3H,5H)-Pyrimidinetrione,5-[(2,3-dihydro-6-methyl-2-oxo-1H-benzimidazol-5-yl)azo]-, Titanium Dioxide, Diketo Pyrrolo-pyrrol, & Cobalt Titanate Green Spinel)
72102-84-2
13463-67-7
84632-65-5
68186-85-6
0 – 5
10 – 15
0 – 5
20 – 25

PSTE Red

PSTE Red Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
345
Pantone
7526 C
R: 138
G: 57
B: 27
Pigment Red 101
(Iron Oxide)
1309-37-1 41
346
Pantone
2347C
R: 225
G: 6
B: 0
Pigment Red 254
(3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione)
84632-65-5 17
349
(Fluorescent)
Pantone
7637 XGC
R: 150
G: 47
B: 74
Pigment Red 169
(Fluorescent Pink)
(Rhodamine 6G)
12237-63-7 41
354
Pantone
7633 C
R: 196
G: 164
B: 167
Pigment Red 254
(3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione)
84632-65-5 0 - 5
370
Pantone
207C
R: 165
G: 0
B: 52
Pigment Violet 19
(Quino(2,3-b)acridine-7,14-dione, 5, 12-dihydro-)
1047-16-1 ~ 38
400
Pantone
1675 XGC
R: 173
G: 68
B: 32
Pigment Red 101
(Iron Oxide)
1332-37-2 5 - 15
49801
Pantone
186C
R: 200
G: 16
B: 46
Blend of
Pigment Orange 36, Pigment Red 202, Pigment White 6, & Pigment Red 254
(Benzimidazolone Orange HL, Quinacridone Magenta RT, Titanium Dioxide, & 3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione)
12236-62-3
3089-17-6
13463-67-7
84632-65-5
~ 17
57951
Pantone
4071C
R: 207
G: 135
B: 157
Blend of
Pigment Violet 19, Pigment White 6, & Pigment Red 254
(Quino(2,3-b)acridine-7,14-dione, 5, 12-dihydro-, Titanium Dioxide, & 3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione)
1047-16-1
13463-67-7
84632-65-5
9
Med-NSHCV2096A
Pantone
2347C
R: 225
G: 6
B: 0
Pigment Red 254
(3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione)
84632-65-5 25
Med-4900-3
Pantone
2347C
R: 225
G: 6
B: 0
Pigment Red 254
(3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione)
84632-65-5 17.32
Med1-4900-3-BO
Pantone
1675C
R: 169
G: 67
B: 30
Pigment Red 254
(3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione)
84632-65-5 1 - 3
Red/Brown 344
Pantone
2443C
R: 142
G: 58
B: 34
Pigment Red 101
(Iron Oxide)
1309-37-1 35 - 40
MED-NSHCV2094A
Pantone
1675C
R: 169
G: 67
B: 30
Pigment Red 101
(Iron Oxide)
1309-37-1 40
MED-4800-3
Pantone
2347C
R: 225
G: 6
B: 0
Pigment Red 254
(3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione)
84632-65-5 17.32

PSTE Orange

PSTE Orange Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
062
Pantone
2007 C
R: 224
G: 165
B: 38
Blend of
Pigment Orange 64 &
Pigment Yellow 180
(2,4,6(1H,3H,5H)-Pyrimidinetrione,5-[(2,3-dihydro-6-methyl-2-oxo-1H-benzimidazol-5-yl)azo]- )
&
Butanamide, 2,2'-[1,2-ethanediylbis(oxy-2,1-phenyleneazo)]bis[N-(2,3-dihydro-2-oxo-1H-benzimidazol-5-yl)-3-oxo- )
72102-84-2 & 77804-81-0 < 5
069A
Pantone
717 C
R: 212
G: 93
B: 0
Pigment Orange 79
(Benzoic Acid, 4-((2-Hydroxy-6-sulfo-1-Naphthalenyl)Azo)-,Strontium Slat (2:1))
250640-08-5 < 10
106802
Pantone
2006 U
R: 241
G: 192
B: 104
Blend of
Pigment Red 254, Pigment Yellow 42 & Pigment White 6
(3,6-Bis(4-chlorophenyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione, Yellow Iron Oxide, & Titanium Dioxide)
84632-65-5
51274-00-1
13463-67-7
~ 41
27761
Pantone
144 C
R: 237
G: 139
B: 0
New Formulation Needed X X
MED-4900-4
Pantone
021C
R: 254
G: 80
B: 0
Pigment Orange 64
(2,4,6(1H,3H,5H)-Pyrimidinetrione,5-[(2,3-dihydro-6-methyl-2-oxo-1H-benzimidazol-5-yl)azo]- )
72102-84-2 5 – 10
MED-NSHCV3017A
Pantone
021C
R: 254
G: 80
B: 0
Pigment Orange 64
(2,4,6(1H,3H,5H)-Pyrimidinetrione,5-[(2,3-dihydro-6-methyl-2-oxo-1H-benzimidazol-5-yl)azo]- )
72102-84-2 5 – 10
MED50-4900-4 (Translucent)
Pantone
7514 XGC
R: 216
G: 163
B: 139
Pigment Orange 64
(2,4,6(1H,3H,5H)-Pyrimidinetrione,5-[(2,3-dihydro-6-methyl-2-oxo-1H-benzimidazol-5-yl)azo]- )
72102-84-2 2.5 – 5

PSTE Yellow

PSTE Yellow Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
126H
Pantone
7405 C
R: 242
G: 205
B: 0
Blend of
Pigment Yellow 180 & Pigment White 6
(Butanamide, 2,2'-[1,2-ethanediylbis(oxy-2,1-phenyleneazo)]bis[N-(2,3-dihydro-2-oxo-1H-benzimidazol-5-yl)-3-oxo- & Titanium Dioxide)
77804-81-0
13463-67-7
17
136
Pantone
7758 C
R: 212
G: 195
B: 4
Pigment Yellow 180
(Butanamide, 2,2'-[1,2-ethanediylbis(oxy-2,1-phenyleneazo)]bis[N-(2,3-dihydro-2-oxo-1H-benzimidazol-5-yl)-3-oxo- )
77804-81-0 < 5
144
Pantone
15-0954 TCX
R: 215
G: 157
B: 0
Blend of
Pigment Yellow 119 & Pigment White 6
(Zinc Ferrite Yellow & Titanium dioxide)
68187-51-9
13463-67-7
1 – 3
3 - 5
148
Pantone
606 C
R: 207
G: 181
B: 0
Pigment Yellow 180
(Butanamide, 2,2'-[1,2-ethanediylbis(oxy-2,1-phenyleneazo)]bis[N-(2,3-dihydro-2-oxo-1H-benzimidazol-5-yl)-3-oxo- )
77804-81-0 < 5
MED-4900-5
Pantone
605 C
R: 225
G: 205
B: 0
Pigment Yellow 138
(Quinophthalone Yellow and Lithol Fast Yellow 1090)
30125-47-4 20

PSTE Green

PSTE Green Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
045
Pantone
19-0230 TCX
R: 73
G: 94
B: 53
Pigment Green 17
(Chromium (III) Oxide)
1308-38-9 15 ≤ X < 40
176
Pantone
339 C
R: 0
G: 179
B: 136
Pigment Green 7
(Copper Phthalocyanine Green)
001328-53-6 < 5
178
Pantone
3500 C
R: 0
G: 110
B: 51
New Formulation Needed X X
193
Pantone
3500 C
R: 0
G: 110
B: 51
New Formulation Needed X X
291
Pantone
7732C
R: 0
G: 122
B: 62
Pigment Green 50
(Cobalt Titanate Green Spinel)
68186-85-6 25 - 50
46231
Pantone
P 154-8C
R: 106
G: 171
B: 61
Pigment Green 50
(Cobalt Titanate Green Spinel)
68186-85-6 5 - 10
Med NSHCV5112E
Pantone
7733C
R: 0
G: 112
B: 65
Blend of
Pigment White 7, Pigment Green 7, & Pigment Yellow 42
(Titanium Dioxide, Phthalocyanine Green, & Iron Hydroxide Oxide Yellow)
13463-67-7
1328-53-9
51274-00-1
5 ≤ X < 15
5 ≤ X < 15
12 ≤ X < 22
Med 4900-6
Pantone
3292
R: 0
G: 89
B: 79
Pigment Green 7
(Copper Phthalocyanine Green)
001328-53-6 9.21
Med2-4900-6
Pantone
18-6031 TCX
R: 0
G: 114
B: 59
Information Needed from Nusil X X

PSTE Blue

PSTE Blue Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
19221
Pantone
P 110-8 C
R: 0
G: 103
B: 158
New Formulation Needed X X
278
Pantone
2728 XG C
R: 0
G: 64
B: 173
Pigment Blue 28
(Cobalt Aluminate)
1345-16-0 25 ≤ X ≤ 50
292
Pantone
5445 C
R: 183
G: 201
B: 211
Pigment Blue 28
(Cobalt Aluminate)
1345-16-0 1 ≤ X ≤ 3
300
Pantone
3025C
R: 0
G: 79
B: 113
New Formulation Needed X X
327
Pantone
16-5114 TCX
R: 100
G: 155
B: 158
New Formulation Needed X X
49591
(Metallic)
Pantone
19-4039 TCX
R: 61
G: 94
B: 140
Blend of
Pigment Black 11, Pigment Blue 15:3, Pigment Red 202, & Pearlescent Pigment
(Black Iron Oxide, Phthalocyanine Blue, Quinacridone Magenta, & Mica Substrate)
1317-61-9
147-14-8
3089-17-6
12001-26-2
~ 25
51602
Pantone
2211C
R: 111
G: 155
B: 164
New Formulation Needed X X
54421
(Sparkles)
Pantone
16-4010 TCX
R: 140
G: 157
B: 173
Blend of
Pigment Black 11, Pigment Blue 15:3, & Pearlescent Pigment
(Black Iron Oxide, Phthalocyanine Blue & Mica Substrate)
1317-61-9
147-14-8
12001-26-2
~ 15
Dark Med-4900-7
Pantone
2765 C
R: 32
G: 21
B: 71
Pigment Blue 15:2
(Copper Phthalocyanine Blue)
12239-87-1 24.91
Med 1-4800-7
Pantone
2728 XGC
R: 0
G: 64
B: 173
Pigment Blue 28
(Cobalt Aluminate)
1345-16-0 40
Med 1-4900-7
Pantone
2728 XGC
R: 0
G: 64
B: 173
Pigment Blue 28
(Cobalt Aluminate)
1345-16-0 40
Med51-4800-7
(Translucent)
Pantone
537 C
R: 187
G: 199
B: 214
Pigment Blue 28
(Cobalt Aluminate)
1346-16-0 1.2
Med51-4900-7
(Translucent)
Pantone
537 C
R: 187
G: 199
B: 214
Pigment Blue 28
(Cobalt Aluminate)
1346-16-0 1.2

PSTE Violet

PSTE Violet Description CAPSURE Color Meter
Reading (Pantone Color)
sRGB Scale Ingredient Name CAS Reg. No. % Pigment (Dry Weight)
367
Pantone
228 C
R: 137
G: 11
B: 88
Pigment Red 202
(2,3-Dichloroquinacridone)
3089-17-6 < 6
369
Pantone
P95-13 C
R: 123
G: 96
B: 136
Blend of
Pigment Blue 28 & Pigment Red 202
(Cobalt Aluminate & 2,3-Dichloroquinacridone)
1333-88-6
3089-17-6
< 5
415
Pantone
2356 C
R: 114
G: 0
B: 97
Blend of
Pigment Violet 19 & Pigment Blue 28
(Quino(2,3-b)acridine-7,14-dione, 5, 12-dihydro- & Cobalt Aluminate)
1047-16-1
1333-88-6
< 5
< 10

 

Contact Our Engineers Today to discuss your LSR coloring needs and receive detailed specifications for our available color options.