- Hardness
- Resistance of rubber to forced distortion as measured by the indentor point of a durometer gauge.
- Hardness
- Shore A: Durometer reading in degrees of rubber hardness as measured on a Shore A gauge. Scale is 0-100, with higher numbers indicating greater hardness.
- Hermetic Seal
- An airtight seal.