The new addition to the Seal Design Guide includes Inspection Specifications – a list of specifications vs. maximum allowable dimensions for various defects. These are great reference tools when setting up part specifications.
Some of these specifications include:
• Foreign Material/Inclusions, contamination in the material or indentation left by removal
• Off-Register misalignment and Mismatch of cross sections
• Backrind, or tearing at the mold parting line
• Non-Fill/Mold Deposit
…and more.
Each section within the Troubleshooting and Inspection Specifications chapter include digital references in PDF format for simple overviews and helpful charts. Open the file and save it for future reference, or bookmark the Seal Design Guide on applerubber.com for easy access online!