Apple Rubber's AppleLabTM Advanced Testing Laboratory
Apple Rubber's AppleLabTM advanced testing laboratory is testimony to our commitment to the highest level of product quality and customer satisfaction possible. Through AppleLab we can assure that your requirements are met or surpassed with:
- Complete PPAP, PPQ, Statistical data to meet your QC requirements.
- One of the most stringent quality assurance programs in the industry
- Process, material and dimensional certification
- Quality assurance that can be documented to your specifications
High Quality Through High Tech
Upon request, Apple Rubber can customize a quality program to meet your specific testing requirements. AppleLab has some of the most sophisticated testing equipment and systems available today. Systems used in our custom testing procedures include:
- Mitutoyo® Quick Vision Measuring System - This non-contact measuring equipment uses the latest optical, video and image processing technologies to accurately measure parts without distortion. Measures even the most demanding microminiature parts quickly and accurately and provides statistical process control data.
- FTIR (Fourier Transform Infrared Spectrophotometer) - Determines chemical make-up of rubber compounds both before and after molding, in a matter of minutes. This ensures the consistency of rubber compounds and seals batch to batch, shipment to shipment.
- Thermogravimetric Analyzer (TGA) - Accurately determines the relative chemical content of materials and their thermal stability at temperatures up to 1,000°C. Completely computer controlled, the TGA delivers unequaled accuracy for material analysis.
- ASTM D1171 - Ozone Testing
AppleLab features a wide variety of other specialized equipment to perform a range of tests on seals such as:
- Tensile strength
- Elongation
- Modulus of elasticity
- Specific gravity
- Swell
- Mettler Analytical Balance - Determines the density of rubber compounds per ASTM Method D297
- (2) MTS Tensile Testers - Determines physical properties of cured rubber compounds per ASTM Method D412
- Tech Pro Tensitech 3 Pull Station - Determines physical properties of cured rubber compounds
- Mittutoyo Optical Comparator - Determines certain dimensional characteristics of various molded rubber products
- Micro-Vu Vision Measuring Machine - Verifies dimensional characteristics of rubber molded products and molds
- Mittutoyo Surface Roughness Tester - Determines surface finish on metal products prior to molding rubber to them
- Shore and Rex Durometer Testers - We have both hand-held and table top testers - Type A for measurement to ASTM D2240 and table top Type M for testing cured rubber of slabs and molded products
- Perkin Elmer FTIR - Used for determining chemical properties of rubber compounds both before and after molding
- Alpha Technologies Production Process Analyzer PPA 2000 - Used to evaluate characteristics of raw material, their vulcanization processes, and their post-vulcanization properties.
- Mast Ozone Test Chamber - ASTM D518, D1171, D1149 Ozone cracking and resistance surface, ozone cracking resistance in a laboratory chamber
- Environtronics Temp/Humidity Chamber - ASTM F1087 - stability of gasket material to linear dimensional change due to hygroscopic expansion/contraction test
- TA Instruments TGA - Thermogravimetric Analyzer - Temperature analysis of rubber compounds for both research and quality control purposes including composition and consistency
- TA Instruments DSC - Differential Scanning Calorimeter - Measurement of temperature and heat flow associated with transition points in materials as a function of time and temperature
- Benz Brittleness Tester - ASTM D2137 - Determine the brittle point of rubber compounds
- ScienTemp Freezer - Cold bend testing of rubber compounds for military applications
- Basler Autogage - Verifies dimensional characteristics of rubber molded parts
ASTM Testing Methods
- ASTM D395 - Compression Set Test, Rubber Products
- ASTM D412 - Tension Properties of Vulcanized Thermostat Rubbers and Thermoplastic Elastomers
- ASTM D471 - Volume Change, Effects of Liquid Test
- ASTM D573 - Deterioration in an Air Oven
- ASTM D624 - Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
- ASTM D865 - Deterioration by Heating in Air
- ASTM D1414 - Complete Testing of O-rings
- ASTM D2137 - Brittleness Temperature - Low - Used to Find the Brittleness Point of Flexible Polymers
- ASTM D2240 - Durometer Hardness