A seal combining the structural advantages of metal or plastic with the sealing advantages of elastomers.
A four-lobed profile primarily used in dynamic situations because of reduced friction and increased resistance to spiral failure. The parting line is located away from the sealing surface, unlike O-rings in radial applications.