LSR parts and seals exhibit a wide temperature range (-75°C to +225°C), low compression set, and resistance to the damaging effects of sunlight and ozone. Available in a durometer range of 10-80 Shore A for virtually any type seal or part including O-rings, gaskets, face seals, housing seals, filter seals®, and custom shapes.