NATURAL RUBBER

ASTM D1418 Designation: NR

ASTM D2000/SAE J200 Type, Class: AA

Apple Compound Designation: NA

Standard Color: Black

Description: Natural Rubber is the vulcanized product of the juice of the Hevea tree (latex).

Key Use(s): Seals in brake systems. Seals in food & beverage applications. Most popular material for non-hydraulic sealing applications. Mainly used for dampeners due to its ability to absorb vibration.

Temperature Range: Standard Compound: -60° to +220°F. (Dry Heat Only)

Hardness (Shore A): 40 to 90.

   