M
MemoryAbility of an elastomeric material to return to its original size and shape after deformation.
MILAbbreviation for Military.
MIL STDMilitary Standard.
MismatchUnequal O-ring cross-sectional radii caused by dimensional differences in the mold cavity.
ModulusThe tensile stress force in p.s.i. required to produce a specified increase in material length (usually 100% elongation).
Modulus of ElasticityOne of several measurements of stiffness or resistance to deformation.
MoldTypically made from steel. Product is formed within machined cavity.
Mold CavityHollow space of the mold within which the uncured rubber compound is shaped and cured to the desired finished product form.
Mold FinishThe surface finish of the mold which imparts the desired surface quality to the finished molded product.
Mold MarksSlight irregularities in the surface of molded articles caused by mold machining marks,or damage to the mold itself.
Mold ReleaseA lubricant used to assist in the removal of rubber products from the mold.
MSAbbreviation for Military Standard.
|