Apple Rubber Products achieved AS9100 certification, the new quality standard of the aerospace industry. AS9100 was designed to build upon and enhance the requirements of IS0 9001, the internationally recognized standard for basic quality management, by focusing on the additional, more rigorous expectations and requirements of the aerospace industry. The certification confirms that Apple Rubber possesses an aerospace quality system that is both consistent and robust, ensuring product, process and service safety, reliability and quality. AS9100 certification is rapidly becoming a prerequisite for doing aerospace business, as many original equipment manufacturers will only work with a handful of suppliers, such as Apple Rubber, who are registered to this standard. These quality requirements are extremely important to aerospace OEMs, which maintain high levels of liability for their product quality. Click on the image above to view our
AS9100B Certificate of Registration |
O-RING RULE OF THUMB #8
Avoid using graphite-loaded compounds with stainless steel, as they tend to pit the stainless seal surface over time. » Learn More

AS9100B