Get the advantages of silicone from Apple Rubber
No other material can match silicone's combination of unique characteristics. This makes it one of the most versatile materials for a wide variety of sealing applications in many industries.
- Unmatched Temperature Resistance - withstands temperature extremes from -75°C to 225°C (-103°F to 437°F).
- Excellent Mechanical Properties - excellent flex resistance, good tensile, tear and elongation strength, and superior compression set resistance, with durometer range of 10-80 Shore A.
- Superior Insulating Properties - exceeds all elastomers in its insulating properties making it ideal for electrical applications. It is non-conductive and maintains dielectric strength in high and low temperature extremes.
- Exceptional Weather Resistance - resists the damaging effects of UV light, ozone, O2, weather, moisture and steam with outstanding aging characteristics.
- Good Chemical Resistance - resists water and many chemicals such as acids, oxidizing chemicals, ammonia and isopropyl alcohol.
- Excellent Dimensional Stability - offers excellent accuracy and provides versatility of shape and form to many seals and parts, even intricate shapes.
Silicone is the remedy for medical applications.
As an example of its advantages, silicone demonstrates superior performance properties for use in medical devices.
- Excellent compatibility with human and animal tissue and body fluids - does not irritate skin or other organs.
- Is extremely soft and pliable, easily conforms to different shapes.
- Biologically inert - Does not support the growth of bacteria
- Does not stain or corrode other materials which it contacts.
- Withstands Autoclave, ETO, and Gamma Sterilization
Apple Rubber has your silicone solutions.
Apple Rubber has the experience, the products and the design engineering capabilities to deliver the exact silicone solution for your applications.
- Extensive range of silicone seals and parts -- O-rings, gaskets, face seals, housing seals, filter seals, microminiature seals, custom shapes, and more.
- More than 30 years of seal experience.
- Durometer range of 10-80 Shore A.
- Any color available.
- FDA, ISO 10993 or USP Class 6 grades available
- Composite seals combining silicone with plastic, metal or mesh material.
- Advanced production systems.
- ISO 9001:2000 Certified.
For more information, call us at 1-800-828-7745.
|
O-RING RULE OF THUMB #11
Static seal cross-sections are generally compressed from 10% to 40%, whereas dynamic seals are from 10% to only 30%. » Learn More
|