Solutions for Plasticizer Extraction

Failure Pattern
Occurring in both static and dynamic seals, primarily in fuel system service, plasticizer extraction is marked by loss of physical volume.

Problem Sources
Extraction of plasticizer by system chemicals.

Suggested Solutions
Employ chemically compatible O-ring material (see Chemical Compatibility Table, Section 6 in the Seal Design Guide).

O-RING RULE OF THUMB #4

Static applications are more tolerant of material and design limitations than dynamic applications. » Learn More

 